Please use this identifier to cite or link to this item: http://repositorio.lnec.pt:8080/jspui/handle/123456789/1010575
Title: Durability of an epoxy adhesive used in civil structural applications
Authors: Sousa, J.
Correia, J. R.
Cabral-Fonseca, S.
Keywords: Structural adhesive;Epoxy;Durability;Hygrothermal ageing;Outdoor ageing
Issue Date: Nov-2017
Publisher: Elsevier
Citation: https://doi.org/10.1016/j.conbuildmat
Abstract: This paper presents an experimental study about the durability of a cold curing structural epoxy (EP) adhesive exposed to different hygrothermal and outdoor ageing environments, typical of civil engineering applications, for up to two years: water and salt water immersion at 20 °C and 40 °C, continuous condensation at 40 °C, and outdoor ageing in a mild Mediterranean climate. After specific exposure periods, changes in the following physical properties and mechanical behaviour of the adhesive were assessed: (i) media diffusion, through water uptake (in hygrothermal environments); (ii) viscoelastic behaviour, through dynamic mechanical analyses (DMA); and (iii) flexural and (iv) in plane shear behaviour. Regarding media diffusion, water uptake did not follow a Fickian behaviour and a final saturation stage was not reached; two alternative non Fickian analytical models were successfully fitted to the test data and the corresponding diffusion parameters were determined. In what concerns the viscoelastic behaviour, while continuous condensation and outdoor ageing caused negligible changes, the Tg of the adhesive generally decreased due to immersion (around 20% in water and 10% in salt water after two years); in addition, at later stages of water immersion, the tan  curve showed significant shape differences, with the usual curve peak being replaced by two different peaks; a generalised reduction of the storage modulus at the glassy plateau was also noted. In terms of mechanical performance, such plasticization effects were visible in the flexural and shear stress strain behaviours. The flexural properties exhibited irreversible degradation, with the highest reductions (two years of ageing in water at 40 °C) being about 24% and 30% in strength and modulus, respectively. Regarding the shear properties, in hygrothermal environments the shear modulus showed similar decreasing trends to the flexural modulus (43% reduction after one year), but the shear strength increased (~25%); the outdoor ageing affected the shear properties in the same way, but the magnitudes of the changes were lower.
URI: https://repositorio.lnec.pt/jspui/handle/123456789/1010575
Appears in Collections:DM/NMO - Comunicações a congressos e artigos de revista

Files in This Item:
There are no files associated with this item.


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.